Differential Scanning Calorimetry Testing

Test

DSC Scan

Property

  • Glass Transition Temperature (Tg)
  • Melting Temperature (Tm)
  • Crystallization Temperature (Tc)

Instrument

  • TA Instruments Model Q200 Modulated Differential Scanning Calorimeter (DSC) with  ‐50 °C to +725 °C temperature capability
    • Mass Flow Control
    • RCS90 Refrigerated Cooling System
    • Gas Dryer

Setup Fees & Conditions

  • Setup Fee
    • Required: Once per batch
    • Price: Included

    Standard

    • ASTM D7426‐08; D3418‐08; E1356‐08
      • Duplicate Scan Up to 100 °C 10 °C/min or Higher Rate
      • Samples: 1
      • Price: $350
    • ASTM D7426‐08; D3418‐08; E1356‐08
      • Duplicate Scan Up to 300 °C 10 °C/min or Higher Rate
      • Samples: 1
      • Price: $410
    • ASTM D7426‐08; D3418‐08; E1356‐08
      • Duplicate Scan Up to 500 °C 10 °C/min or Higher Rate
      • Samples: 1
      • Price: $470